Research Article

Preclinical Testing of New Hydrogel Materials for Cartilage Repair: Overcoming Fixation Issues in a Large Animal Model

Figure 6

μCT scans of osteochondral trochlea defects 12 weeks after implantation of different hydrogels. μCT visualization revealing bone lysis in all groups, scale bar: 2 mm (a). Bone volume/total volume was quantified in a volume of interest for each defect, and there was no statistical significance between the groups (b). To depict the loss of bone volume, BV/TV was compared to day 0 confirming more severe bone loss in defects treated with PCL-reinforced constructs compared to empty control defects. Mean percentage of bone loss ± SD per group compared to day 0 defects. : vs. empty control (ANOVA) (c).
(a)
(b)
(c)