Research Article
Turning the Cocopith Waste into Myceliated Biocomposite to Make an Insulator
Table 6
Biocomposite tensile strength.
| No. | Specimens | Thickness (mm) | Area (mm2) | Max load (N) | Extension (mm) | Tensile strength (MPa) | Elongation (%) |
| 1 | Biocomposite 1 | 4.35 | 43.94 | 5.25 | 0.11 | 0.12 | 0.27 | 2 | Biocomposite 2 | 4.00 | 40.00 | 4.14 | 0.14 | 0.1 | 0.32 | 3 | Biocomposite 3 | 3.9 | 37.44 | 2.15 | 0.11 | 0.57 | 0.27 |
|
|