ANOVA test comparing degradation process and roughness over mechanical strength (MPa) at 450% strain, mechanical strength (MPa) at rupture, and deformation at rupture.

PropertyMechanical strength at rupture (MPa)Mechanical strength at 450% strain (MPa)Deformation at rupture (%)

Roughness0.6520.8990.724
Degradation process0.0020.0010.004