Research Article

Breakdown and Evolution of the Protective Oxide Scales of AISI 304 and AISI 316 Stainless Steels under High-Temperature Oxidation

Figure 8

(a) SEM micrograph of the cross-section of the AISI 304 stainless steel oxidized at 1000°C for 100 hours and (b) XRD mapping analysis of the line shown.
824676.fig.008a
(a)
824676.fig.008b
(b)