Research Article

Analysis of Short-Term Steel Corrosion Products Formed in Tropical Marine Environments of Panama

Table 2

Starting date of exposure to the atmosphere.

Test siteā€‰Type of steelā€‰
A-36A-588COR 420

Tocumen01/30/0701/30/0707/24/07
Sherman-Open02/02/0702/02/0707/23/07
Sherman-Coastal02/02/0702/02/0707/23/07
Sherman-Breakwater01/31/0701/31/0707/23/07