Research Article
Analysis of Short-Term Steel Corrosion Products Formed in Tropical Marine Environments of Panama
Table 4
Two year results of the corrosion rates (μm y−1).
| Exposure time (months) | Tocumen | Sherman-Open | Sherman-Coastal | Sherman-Breakwater | A-36 | A-588 | COR 420 | A-36 | A-588 | COR 420 | A-36 | A-588 | COR 420 | A-36 | A-588 | COR 420 |
| 3 | 22.1 | 33.3 | 63.7 | 31.6 | 37.2 | 51.2 | 47.3 | 52.7 | 67.1 | 1011.4 | 801.0 | 177.9 | 6 | 41.8 | 38.8 | 48.0 | 33.9 | 44.5 | 55.0 | 42.5 | 42.3 | 67.1 | 963.0 | 664.2 | 358.6 | 9 | 38.1 | 39.1 | 34.1 | 36.8 | 37.4 | 29.3 | 37.0 | 36.0 | 44.6 | 771.0 | 504.3 | 456.6 | 12 | 38.5 | 35.2 | 38.3 | 42.2 | 36.6 | 39.8 | 48.9 | 40.9 | 42.6 | 718.8 | 469.3 | 473.1 | 24 | 24.4 | 37.2 | 19.6 | 26.7 | 22.2 | 17.5 | 40.2 | 29.9 | — | 654.6 | 561.8 | 523.6 |
|
|