Six-Year Evaluation of Thermal-Sprayed Coating of Zn/Al in Tropical Marine Environments
Figure 4
Thermal-sprayed coating of Zn/Al by flame process, sealed with wash primer (445 μm). (a) 12 months of exposure. (b) 24 months of exposure. (c) 36 months of exposure. (d) 48 months of exposure.