Research Article

Environmental and Material Influences on the Stress-Corrosion Cracking of Steel in H2O–CO–CO2 Solutions

Figure 5

Reduction in area and elongation as a function of pressure of slow strain-rate tests performed at C with a gas mixture of 25% CO and 75% CO2.
414156.fig.005