Morphology of Al after anodic oxidation for 5 min at 0.3 V nobler than the pitting corrosion potential in a solution containing 0.1 mol·dm−3 of Na2SO4 and 300 ppm of Cl. (a, b) Pure Al without ECAP. (c, d) Pure Al with ECAP.