Research Article

Deposition of Cerium-Based Conversion Coatings on Aluminum Alloy 380

Figure 4

(a) Potentiodynamic polarization curves and (b) impedance spectra for CeCCs deposited AA 380 substrates rinsed at 100°C as a function of coating deposition time.
760284.fig.004a
(a)
760284.fig.004b
(b)