Corrosion Behaviour of a Highly Alloyed Austenitic Alloy UB6 in Contaminated Phosphoric Acid

Figure 5

Mott-Schottky curves for the passive films formed in contaminated 5.5 M phosphoric acid at 20°C, 40°C, 60°C, and 80°C at the formation potential of .