Research Article

Combating Corrosion Degradation of Turbine Materials Using HVOF Sprayed 25% (Cr3C2-25(Ni20Cr)) + NiCrAlY Coating

Figure 11

SEM and EDX analysis of 25% (Cr3C2-25(Ni20Cr)) + NiCrAlY coated materials subjected to hot corrosion for 50 cycles in Na2SO4 + 50%V2O5 at 800°C. (a) Ti-31, (b) Superco-605, and (c) MDN-121.
824659.fig.0011a
(a)
824659.fig.0011b
(b)
824659.fig.0011c
(c)