Corrosion of Steel in High-Strength Self-Compacting Concrete Exposed to Saline Environment

Table 3

Self-compacting features.

SymbolSP %w/c or w/cmSelf-compacting features
TestsActual value

R0.52Slump180 mm

SP30.31Slump flow
50 cm
-ring flow Passing ability
-funnel time
710 mm
7 sec
700 mm
13 mm
8 sec

SF-R30.31Slump flow
50 cm
-Ring flow
Passing ability
-funnel time
683 mm
7 sec
670 mm
13 mm
9 sec

SF-A30.31Slump flow
50 cm
-Ring flow
Passing ability -funnel time
675 mm
8 sec
660 mm
15 mm
9 sec