Simulation of the Relaxation Potential Profile of an ac-dc-ac Test
Figure 10
Time constants and as functions of porosity with the bulk NaCl concentration as a parameter. The bulk conditions were pH 9 and M Al3+, the applied dc potential was −1.9 V, and the coating was 0.2 mm thick.