Research Article
Effect of High Temperature Sodium Hydroxide Immersion on Fusion Bond Epoxy Coating
Figure 2
SEM cross section analysis of Fusion Bond Epoxy coating: (a) before and (b) after exposure to 5% NaOH solution for 30 days at 93°C/200°F.
(a) Before exposure |
(b) After exposure |