Research Article
Effect of High Temperature Sodium Hydroxide Immersion on Fusion Bond Epoxy Coating
Figure 9
DSC scans of FBE coating system: (a) before exposure and after exposure to 5% NaOH solution for 30 days at 93°C/200°F (b) discolored zone, and (c) unaffected underlying zone.
(a) Before exposure |
(b) Discolored zone |
(c) Unaffected underlying zone |