Research Article

Electrochemical and Microstructural Analysis of FeS Films from Acidic Chemical Bath at Varying Temperatures, pH, and Immersion Time

Figure 2

P-XRD analysis on the 4130 alloy surface at (a) 50°C, 4 pH, and 48 hours, (b) 25°C, 4 pH, and 24 hours, (c) 50°C, 2 pH, and 24 hours, (d) initial condition (uncorroded sample), and (e) 75°C, 4 pH, and 24 hours.
(a)
(b)
(c)
(d)
(e)