Research Article

Electrochemical and Microstructural Analysis of FeS Films from Acidic Chemical Bath at Varying Temperatures, pH, and Immersion Time

Figure 3

SEM analysis of corrosion products of 4130 alloy after (a) 24-, (c) 48-, and (e) 72-hour immersion at pH 4 and 50°C and EDX analysis of corrosion products of 4130 alloy after (b) 24-, (d) 48-, and (f) 72-hour immersion at pH 4 and 50°C.
(a)
(b)
(c)
(d)
(e)
(f)