Research Article

Electrochemical and Microstructural Analysis of FeS Films from Acidic Chemical Bath at Varying Temperatures, pH, and Immersion Time

Figure 9

SEM image of corrosion products on surface of 4130 alloy after 24-hour immersion at pH 4 and 50°C.