Mix design of concrete.

MaterialUnit Weight (kg/m3)
20 MPa30 MPa40 MPa

Slump (cm)
Cement395468535
Crushed stone12221085870
Sand605700750
Free water205205210
Water–cement ratio (%)52440.39
Gmax (mm)202020
(%)323945
Calcium stearate0, 1, 5, 100, 1, 5, 100, 1, 5, 10