The quantity of specimens.
| No | Code | Quality of concrete (MPa) | Quantity of specimens | Compressive strength | Infiltration of chloride ions |
| 1 | St-0.00-20 | 20 | 3 | 3 | 2 | St-0.25-20 | 20 | 3 | 3 | 3 | St-1.27-20 | 20 | 3 | 3 | 4 | St-2.53-20 | 20 | 3 | 3 | 5 | St-0.00-30 | 30 | 3 | 3 | 6 | St-0.21-30 | 30 | 3 | 3 | 7 | St-1.07-30 | 30 | 3 | 3 | 8 | St-2.48-30 | 30 | 3 | 3 | 9 | St-0.00-40 | 40 | 3 | 3 | 10 | St-0.19-40 | 40 | 3 | 3 | 11 | St-0.90-40 | 40 | 3 | 3 | 12 | St-1.87-40 | 40 | 3 | 3 |
|
|