Wet Oxidation Behavior of Near-Stoichiometric SiC Fibres in the Simulated Aeroengine Circumstance
Figure 3
The XRD patterns of KD-S fibres after annealing for 1 h. (a) Under simulated atmosphere. (b) Under simulated atmosphere and under dry air.