Study on the Electrochemical Performance of Sacrificial Anode Interfered by DC Stray Current
Table 4
The corrosion electrochemical parameters of the anode at different ambient temperature.
| Experiment days (d) | Ambient temperature (V) | Cathodic slope | Anodic slope | Polarization resistance (Ωcm2) | Corrosion current density (μA/mm2) |
| 0 | 10°C | -5.234 | 4.802 | 2.208 | 1.85 | room- temperature | -5.131 | 4.834 | 2.184 | 2.19 | 30°C | -4.954 | 4.153 | 2.177 | 2.31 |
| 2 | 10°C | -4.738 | 5.027 | 3.688 | 1.47 | room- temperature | -5.072 | 5.106 | 3.670 | 1.62 | 30°C | -4.931 | 5.274 | 2.781 | 1.63 |
| 4 | 10°C | -5.215 | 5.723 | 4.693 | 0.92 | room- temperature | -4.641 | 5.0821 | 4.599 | 0.98 | 30°C | -4.624 | 5.023 | 3.593 | 1.11 |
| 6 | 10°C | -5.378 | 5.615 | 5.857 | 0.76 | room- temperature | -4.713 | 5.026 | 5.775 | 0.83 | 30°C | -4.858 | 4.964 | 3.876 | 1.02 |
| 8 | 10°C | -5.495 | 6.362 | 6.439 | 0.71 | room- temperature | -4.724 | 5.118 | 6.379 | 0.71 | 30°C | -4.582 | 4.954 | 4.068 | 0.75 |
|
|