Research Article

Hot Corrosion of SrTiO3 Perovskite in Na2SO4 + 50 wt.% V2O5 and Na2SO4 + 10 wt.% NaCl Environments at 900°C

Figure 5

Surface morphology of SrTiO3 after being subjected to hot corrosion in Na2SO4 + 50 wt.% V2O5 environment at 900°C. A porous layer and corrosion products were observed on the surface.