Effect of Aging Treatment on Intergranular Corrosion Properties of Ultra-Low Iron 625 Alloy
Table 3
Composition at some topical points, as obtained by EDS analysis (wt%).
| Position | Ni | Cr | Mo | Nb | Ti | C |
| 1 | 57.03 | 13.57 | 8.33 | 11.89 | 1.70 | 7.47 | 2 | 58.50 | 15.25 | 8.84 | 10.00 | 2.18 | 5.22 | 3 | 55.79 | 15.75 | 13.01 | 7.60 | - | 7.85 | 4 | 67.11 | 17.91 | 7.78 | 3.57 | - | 3.62 | 5 | 41.42 | 39.35 | 8.83 | - | 2.31 | 8.09 | 6 | 65.59 | 7.54 | 8.56 | 9.97 | 2.56 | 5.77 | 7 | 41.65 | 16.00 | 30.22 | 2.42 | - | 9.71 | 8 | 67.51 | 17.43 | 7.64 | 2.37 | - | 5.04 |
|
|