Research Article
Investigation of Mild Steel Corrosion in the Cement Production Associated with the Usage of Secondary Fuels
Figure 16
Single polarisation measurements under varied aeration conditions at ambient temperature recorded after 0.5-1 h of immersion in 0.1 M KCl electrolyte solution from cathodic () to anodic with 1 mV/s; inserts: corresponding Stern-Geary corrosion data (mean values).