Open circuit potentials (mean values at 200 s after immersion start of three measurements each) for 1 M KCl electrolyte solution.

Conditionocp (mV)

Ambient temp., aerated, unstirred-610
40 °C, aerated, unstirred-637
Ambient temp., pressurised-air purge-530
Ambient temp., N2 purge-599