Corrosion kinetic parameters , , and coefficient of .

Test stationSMSMA
No.Location (μm) (μm)

T1Mawlamyine15.090.650.9214.630.940.91
T2Yangon17.320.520.8616.570.600.74
T3Mandalay8.920.420.916.760.540.97