Research Article

Examination of Perovskite Structure CaMnO3-δ with MgO Addition as Oxygen Carrier for Chemical Looping with Oxygen Uncoupling Using Methane and Syngas

Table 6

Oxygen concentration at the end of the CLOU period for tested oxygen carrier particles.

NotationMolar compositionSintering temperatureConc. ( ) end of inert  ( = 900°C)
(°C)Before fuelAfter fuel
(%)(%)

5.6% MgOCaMn0.8Mg0.2O312000.50.1
13000.40.3

2.7% MgOCaMn0.9Mg0.1O312000.50.3
13000.50.4