Total weight loss of all samples.

SamplePET + 0 g EGPET + 0.4 g EGPET + 0.6 g EGPET + 1 g EGPET + 1.4 g EGPET + 2 g EG

Decomposition temperature (°C)374.64374.71374.71374.71374.71374.71
% weight loss0.732.592.814.374.895.42
% moisture content @ 100°C0.100.020.120.180.12