Thermal gravimetric data of DNDC (A0) and the OC products.

SampleVolatile content (%)Degradation temperature (°C)Weight loss at final stage (%)
Initial stageFinal stage

DNDC (A0)5.7434877.99
OC-6 hrs (D1)9.1421835172.85
OC-12 hrs (D2)9.68186, 22334572.80
OC-24 hrs (A4)9.87182, 22034172.73
OC-36 hrs (D3)11.73178, 22333471.83