Research Article
Study on Susceptibility and Mechanism of Reheat Cracking in Welded Joint of Type 347 Austenitic Stainless Steel
Figure 11
Appearance of fractured SSRT test specimens. (a) M-L7 at 750°C, (b) M-L6 at 800°C, (c) M-L4 at 850°C, (d) M-L1 at 900°C.
(a) |
(b) |
(c) |
(d) |