Study on Susceptibility and Mechanism of Reheat Cracking in Welded Joint of Type 347 Austenitic Stainless Steel

Table 3

Welding parameters.

Specimen no.Weld layerWelding methodPolarityWelding current (A)Welding voltage (V)Welding speed (cm·min−1)Heat input (KJ·cm−1)

M1GTAWDCSP100∼12012∼135.0∼5.514.4∼15.8
2SMAWDCRP100∼11025∼279∼1017∼19
Other layersSMAWDCRP100∼11025∼279∼1017∼19