Research Article

Microleakage after Thermocycling of Three Self-Etch Adhesives under Resin-Modified Glass-Ionomer Cement Restorations

Table 3

Mean scores of microleakage for RMGIC restorations using a polyacrylic acid conditioning or three different self-etching adhesive systems.

Mean scores of microleakage ( SD)
DC + FIISE + FII

GROUP IDC-1 + FII-11.49 ( 0.94)XIII + FII0.81 ( 0.76)* .0001
( )( )
GROUP IIDC-2 + FII-20.64 ( 0.68)iB exp + FII0.81 ( 0.93)*.43
( )( )
GROUP IIIDC-3 + FII-30.61 ( 0.70)APLP + FII0.69 ( 0.63)*.33
( )( )

TotalAll DC + FII0.91 ( 0.88)All SE + FII0.77 ( 0.78).091
( )( )

*When the different adhesive systems are compared, there is no statistically significant difference between the 3 one-step SE adhesives tested in this study ( ).