Evaluation of the Effect of Water on Three Different Light Cured Composite Restorative Materials Stored in Water: An In Vitro Study

Table 2

The mean weights of three composite specimen measured daily during the first week of the observation.

No. of observationsGroup AGroup BGroup C

Initial20929.2 (28.140)910. 7 (18.979)905. 6 (15.806)
First day20932.5 (26.963)916. 7 (19.074)908. 3 (15.267)
Second day20933.8 (27.976)919. 1 (16.368)910. 0 (15.499)
Third day20936.2 (26.246)921. 2 (15.161)911. 7 (15.291)
Fourth day20938.0 (23.576)922. 8 (15.087)913. 5 (14.855)
Fifth day20940. 4 (25.124)924. 4 (15.916)915. 5 (15.157)
Sixth day20943. 8 (25.614)928. 0 (14.706)917. 5 (14.652)

(standard deviations are given within brackets).