Evaluation of the Effect of Water on Three Different Light Cured Composite Restorative Materials Stored in Water: An In Vitro Study

Table 3

The mean weights of three composite specimen measured daily during the entire period of the observation.

No. of observationsGroup AGroup BGroup C

Initial20929.2 (28.140)910. 7 (18.979)905. 6 (15.806)
First week20943. 8 (25.614)928. 0 (14.706)917. 5 (14.652)
Second week20945. 4 (25.488)929. 5 (14.580)919. 4 (13.808)
Third week20947. 7 (26.725)930. 6 (14.303)920. 3 (13.632)
Fourth week20950. 2 (26.998)931. 2 (14.722)922. 1 (12.377)
Fifth week20953. 3 (28.507)932. 8 (14.388)923. 4 (12.445)
Sixth week20955. 3 (30.479)934. 4 (13.936)924. 5 (12.441)

(standard deviations are given within brackets).