SEM images of Ti-6Al-4V and γ-TiAl alloys. (a), (b): untreated, (c), (d): oxidized at 500°C, (e), (f): oxidized at 800°C, and (g), (h): MAO at 225 mA, 4 mins.
(a)
(b)
(c)
(d)
(e)
(f)
(g)
(h)