Research Article

Titanium Oxide: A Bioactive Factor in Osteoblast Differentiation

Figure 2

SEM micrographs of hFOB 1.19 cells on a glass coverslip (positive control), GTi and TiV (untreated alloys), thermally oxidized TiV5 and GTi5 (500°C), TiV8 and GTi8 (800°C), micro arc oxidized (MAO) TiV (200 mA and 225 mA at 3 min and 4 min), and MAOGTi (200 mA and 225 mA at 3 min and 4 min) disks. Magnification 1000x.