Description of the experimental and commercial materials based on manufacturer’s safety data sheets.

MaterialManufacturerChemistryBatch number

RelyX Luting Plus Automix3M ESPEPaste/paste resin-modified glass-ionomer (RMGI) cement
Methacrylated polyacid, water, fluoroaluminosilicate (FAS) glass, methacrylated monomers, and initiators
L: N305342
EXP: 2013-07

GC FujiCEM AutomixGCPaste/paste RMGI cement
Polyacid, water, FAS glass, methacrylated monomers, and initiators
L: 1003191
EXP: 2012-03

Ketac Cem Aplicap3M ESPEPowder/liquid conventional glass-ionomer cement
Polyacid, water, and FAS glass
L: 400845
EXP: 2013-08

Panavia F 2.0KurarayPaste/paste dual-curing resin-based adhesive cement
10-Methacryloyloxydecyl dihydrogen phosphate (MDP), hydrophobic methacrylated monomers, silanated silica and barium glass fillers, and initiators
L: 61112
EXP: 2013-01

Adper Easy Bond3M ESPESelf-Etch Adhesive
Water, ethanol, methacrylated polyacid, methacrylated monomers, phosphoric acid-6-methacryloyloxy-hexylesters mixture (MHP), silane treated silica, and initiators
L: 418381
EXP: 2012-10

RelyX Ceramic Primer3M ESPECeramic primer
Water, ethanol, and methacryloyloxypropyl-trimethoxy silane
L: N105093
EXP: 2012-08

Experimental compositions3M ESPEPaste/paste dual-curing composite filling
Methacrylated monomers, varying Addition-Fragmentation Monomer (AFM) levels, fillers, and initiators
NA