Effect of Glazing on Flexural Strength of Full-Contour Zirconia
Table 4
Firing steps for glazed firing.
| Glaze material | Idle temp. (°C) | Dry time (s) | End temp. (°C) | Holding time (min) | Heat rate (°C/min) | Vacuum | Tray open (°C) |
| Prettau Zirconia glaze | 350 | 5 | 820 | 2 | 55 | + | — | Zirlux FC glaze | — | 6 | 1000 | 0 | 55 | + | 480 |
|
|