Research Article
Evaluation of Some Mechanical Properties of a Maxillofacial Silicon Elastomer Reinforced with Polyester Powder
Table 1
Descriptive statistics and one-way analysis of variance (ANOVA) for hardness, tear strength, tensile strength, and roughness.
| | N | Mean | Std. deviation | Std. error | 95% confidence interval for mean | Minimum | Maximum | Lower bound | Upper bound |
| Roughness (μm) | 0% | 10 | 0.4507 | 0.03858 | 0.01220 | 0.4231 | 0.4783 | 0.40 | 0.50 | 1% | 10 | 0.4415 | 0.03904 | 0.01234 | 0.4136 | 0.4694 | 0.36 | 0.49 | 3% | 10 | 0.4316 | 0.01891 | 0.00598 | 0.4181 | 0.4451 | 0.41 | 0.46 | 5% | 10 | 0.4822 | 0.06560 | 0.02075 | 0.4353 | 0.5291 | 0.41 | 0.62 |
| Tensile (MPa) | 0% | 10 | 4.8850 | 0.45344 | 0.14339 | 4.5606 | 5.2094 | 4.50 | 5.90 | 1% | 10 | 5.0100 | 0.11547 | 0.03651 | 4.9274 | 5.0926 | 4.91 | 5.21 | 3% | 10 | 4.5900 | 0.38632 | 0.12217 | 4.3136 | 4.8664 | 4.12 | 5.00 | 5% | 10 | 4.4110 | 0.21179 | 0.06697 | 4.2595 | 4.5625 | 4.21 | 4.75 |
| Tear (kN/m) | 0% | 10 | 20.7700 | 2.40557 | 0.76071 | 19.0492 | 22.4908 | 15.50 | 23.60 | 1% | 10 | 23.4800 | 0.76274 | 0.24120 | 22.9344 | 24.0256 | 22.00 | 24.50 | 3% | 10 | 21.9500 | 2.97630 | 0.94119 | 19.8209 | 24.0791 | 19.00 | 27.00 | 5% | 10 | 20.0000 | 0.74536 | 0.23570 | 19.4668 | 20.5332 | 19.00 | 21.00 |
| Hardness (mm) | 0% | 10 | 30.7300 | 1.72501 | 0.54550 | 29.4960 | 31.9640 | 28.10 | 33.10 | 1% | 10 | 31.0400 | 1.72511 | 0.54553 | 29.8059 | 32.2741 | 28.10 | 33.40 | 3% | 10 | 34.3100 | 1.51617 | 0.47946 | 33.2254 | 35.3946 | 33.00 | 38.30 | 5% | 10 | 34.6750 | 1.28609 | 0.40670 | 33.7550 | 35.5950 | 33.20 | 36.70 |
|
|