Mechanical propertiesSum of squaresdfMean squareFSig.

RoughnessBetween groups0.01430.0052.5010.075
Within groups0.069360.002
Total0.08339

TensileBetween groups2.23630.7457.2190.001
Within groups3.717360.103
Total5.95439

TearBetween groups68.958322.9865.8260.002
Within groups142.042363.946
Total211.00039

HardnessBetween groups131.287343.76217.6740.000
Within groups89.140362.476