Research Article
Is Deterioration of Surface Properties of Resin Composites Affected by Filler Size?
Table 1
Composition of materials used in the study.
| Resin composite | Filler particles (ground glass (Ba-Al-B-silicate glass)) | Matrix | Shape | Size (nm) | Wt (%) | Vol (%) |
| I1 | Irregular | 450 | 76.4 | 56.7 | Bis-GMA, UDMA, and TEGDMA | I2 | Irregular | 700 | 76.4 | 56.7 | | I3 | Irregular | 1000 | 76.4 | 56.7 | | I4 | Irregular | 1500 | 76.4 | 56.7 | | I5 | Irregular | 450, 1000 (1 : 3) | 76.4 | 56.7 | | I6 | Irregular | 450, 700, and 1500 (1 : 1:3) | 76.4 | 56.7 | | SP | Spherical | 100 | 72.4 | 56.7 | | Tetric ceram (TC) | | | | | | Lot: C49490 | Irregular & spherical | 40, 200, and 1000 | 79 | 60 | |
|
|