Research Article
Comparison of Marginal and Internal Adaptation in Endocrowns Milled from Translucent Zirconia and Zirconium Lithium Silicate
| | Area | Group | Mean | SD | Min-max | value |
| Internal gap (µm, n = 14) | Pulpal | Zr | 99.75 | ±17.99 | 81.01–145.83 | 0.047 | ZLS | 82.65 | ±24.79 | 58.98–149.38 | Axiopulpal | Zr | 113.81 | ±17.18 | 87.63–148.72 | 0.002 | ZLS | 85.62 | ±25.27 | 54.13–130.88 | Axial | Zr | 78.13 | ±14.67 | 56.71–100.21 | 0.125 | ZLS | 69.09 | ±15.52 | 47.24–98.56 | Axiomarginal | Zr | 56.42 | ±14.00 | 40.51–81.01 | 0.580 | ZLS | 53.35 | ±14.95 | 34.37–86.12 | Overall internal gap | Zr | 87.03 | ±14.39 | 66.46–117.36 | 0.028 | ZLS | 72.68 | ±18.05 | 51.22–112.66 |
|
|
Zr, zirconia; ZLS, zirconium lithium silicate; SD, standard deviation; Min, minimum; Max, maximum.
|