Comparison of Marginal and Internal Adaptation in Endocrowns Milled from Translucent Zirconia and Zirconium Lithium Silicate
Table 3
Mean marginal gaps and standard deviations before cementation (replica and direct view technique), after cementation, and after thermomechanical aging.
Marginal gap (µm, n = 14)
Before cementation replica technique
Before cementation direct view
After cementation direct view
After aging direct view
Group
Mean
SD
Mean
SD
Mean
SD
Mean
SD
Zr
58.33
±8.43
50.52
±7.35
64.02
±8.66
78.52
±10.25
ZLS
54.14
±9.02
47.71
±8.62
61.51
±9.60
80.62
±11.72
value in comparison to precementation direct view measurement
<0.001
<0.001
Zr, zirconia; ZLS, zirconium lithium silicate; SD, standard deviation.