Research Article
Synthesis of a Calcium Silicate Cement Containing a Calcinated Strontium Silicate Phase
Table 2
Comparison of compressive strength (MPa) and setting time (min) of different groups.
| Groups | Compressive strength (mean ± std. deviation) | Setting time (mean ± std. deviation) | Day 1 | Day 7 |
| CSC | 6.91 ± 3.02a | 20.29 ± 8.01b | 138.50 ± 12.48A | CSC/10Sr | 5.01 ± 2.31a | 13.17 ± 3.27b | 127.50 ± 6.77B | CSC/20Sr | 6.46 ± 3.54a | 14.73 ± 7.49b | 129.20 ± 9.70B | CSC/30Sr | 5.71 ± 2.19a | 16.77 ± 7.07b | 95/00 ± 9.13C |
|
|
Different letters indicate presence of a significant difference.
|