Research Article

Surface of Alumina Films after Prolonged Breakdowns in Galvanostatic Anodization

Figure 2

Fragments (50 seconds) of a kinetic curve (Figure 1) at different moments of anodizing (during breakdown).
126726.fig.002a
(a)
126726.fig.002b
(b)