Research Article

Electrochemical Response of Platinum Ultrathin Layer Formed by Pulsed Laser Deposition

Table 2

Pt active area ( ) corresponding to the deposition time calculating by using CVs in 0.5 M sulfuric acid solution as shown in Figure 4.

Sample (cm2)

ULPt(30 s)0.29
ULPt(60 s)0.40
ULPt(90 s)0.88
ULPt(120 s)1.06