Research Article

Photocatalytic Properties of Size-Controlled Titania Nanotube Arrays

Figure 4

Effects of the applied voltage of titania nanotube arrays (TNAs) anodized for 5 h (a) on the degree of MB degradation as a (at 365 nm) with ultra-violet irradiation time, (b) on the correlation between the inner diameter and the apparent rate constant, that is, the slope of (a), and (c) on the apparent rate constant as a function of the length. The size and electric field factors of TNAs for the apparent rate constant of respective voltage regions are summarized in Table 1.
656939.fig.004a
(a)
656939.fig.004b
(b)
656939.fig.004c
(c)