Square wave voltammogram in 0.5 mol L−1 H2SO4 for different phenol concentrations from (a) 30; (b) 50; (c) 70; (dash style) standard solution; (d) 90; (e) 110 and (f) 130 μmol L−1, using BDND electrode. f = 60 Hz, step potential = 2 mV and amplitude = 70 mV. Inset: analytical curve for phenol peak.